SAE AMS7000

Sale!

Original price was: $81.00.Current price is: $40.50.

Laser-Powder Bed Fusion (L-PBF) Produced Parts, Nickel Alloy, Corrosion and Heat-Resistant, 62Ni – 21.5Cr – 9.0Mo – 3.65Nb Stress Relieved, Hot Isostatic Pressed and Solution Annealed
standard by SAE International, 06/08/2018

Category:

Description

This specification covers a corrosion and heat-resistant nickel alloy in the form of parts produced by laser-powder bed fusion (L-PBF) that are subjected to post-deposition stress relief (SR), hot isostatic press (HIP) and solution anneal operations. Parts may require subsequent machining or surface finishing to meet specific application requirements.

Product Details

Published:
06/08/2018
File Size:
1 file , 210 KB